Thermal shock resistant clay bricks for hot blast furnaces
Index |
RN-42 |
HRN-42 |
HRN-48 |
Al2O3 % |
≥42 |
≥42 |
≥48 |
Fe2O3 % |
≤1.7 |
≤1.7 |
≤1.7 |
Fire resistance Refractoriness, ℃ |
≥1750 |
≥1750 |
≥1750 |
Bulk density BD ,g/cm3 |
≥2.15 |
≥2.15 |
≥2.35 |
Apparent porosity % |
≤24/23 |
≤24/21 |
≤24/21 |
Normal temperature compressive strength CSS, MPa |
≥30 |
≥40 |
≥40 |
Softening onset temperature at 0.2 MPa load RUL,℃ |
≥1400 |
≥1520 |
≥1550 |
Reburning line change rate PLC(%) |
0~-0.3 |
0~-0.3 |
0~-0.3 |
TSR ,(1100℃ water cooling)next Cycle |
≥20 |
≥30 |
≥40 |
Note:The denominator value refersto the date of check bricks |
Relevant case
If you are interested in related products, welcome to leave us a message ~
Henan Winna Group Industries Co., Ltd.
Service Hotline:
Address:
Beishankou Town, Gongyi, Henan Province
Copyright©Henan Winna Group Industries Co., Ltd. 豫ICP备2023013320号 Powered by www.300.cn This website already supports IPv6